WMP-VR-R
POLYPROPYLENE / SCRIM / KRAFT
Meets ASTM C1136, Type IV

FACING COMPOSITION DESCRIPTION VALUES (ENGLISH) VALUES (METRIC)
White Film Polypropylene 0.0015 inch 38.1 micron
Adhesive Flame Resistant 4 / inch (MD) 16 / 100 mm (MD)
Reinforcing Tri-directional Fiberglass 4 / inch (XD) 16 / 100 mm (XD)
Film Metallized Polyester 0.0005 inch 12.7 micron

 

PHYSICAL PROPERTIES
TEST METHOD VALUES (ENGLISH) VALUES (METRIC)
Basis Weight Scale 14 lbs / 1000 ft² 68 g / m²
Permeance (WVTR) ASTM E96
Procedure A
0.02 perm
(grains/hr.ft².in Hg)
1.15 ng / N.s
Puncture Resistance ASTM C1136 125 beach units 3.7 Joules
Tensile Strength ASTM C1136 35 lbs/inch width (MD)
35 lbs/inch width (XD)
6.1 kN / m (MD)
6.1 kN / m (XD)
Caliper / Thickness Micrometer 0.007 inch 178 micron
Accelerated Aging 30 Days @
95% RH, 120°F (49°C)
No Corrosion
No Delamination
No Corrosion
No Delamination
Low Temperature Resistance ASTM D1790
-40°F (-40°C)
Remains Flexible
No Delamination
Remains Flexible
No Delamination
High Temperature Resistance 4 hours @
240°F (116°C)
Remains Flexible
No Delamination
Remains Flexible
No Delamination
Water Immersion 24 hours @ 73°F (23°C) No Delamination No Delamination
Mold Resistance ASTM C665 / C1338 No Growth No Growth
Dimensional Stability ASTM D1204 0.25% 0.25%
Light Reflectance ASTM C523 85% 85%

 

FIRE TESTING UL-723 / ASTM E84
  Flame Spread Smoke Developed
Polypropylene Exposed 10 10
Polyester Exposed 15 5