WMP-10
POLYPROPYLENE / SCRIM / KRAFT
Meets ASTM C1136, Type II, IV

FACING COMPOSITION DESCRIPTION VALUES (ENGLISH) VALUES (METRIC)
White Film Metallized Polypropylene 0.0015 inch 38.1 micron
Adhesive Flame Resistant 5 / inch (MD) 20 / 100 mm (MD)
Reinforcing Tri-directional Fiberglass 5 / inch (XD) 20 / 100 mm (XD)
Kraft White 14 lbs / 3000 ft² 23 g / m²

 

PHYSICAL PROPERTIES
TEST METHOD VALUES (ENGLISH) VALUES (METRIC)
Basis Weight Scale 19 lbs / 1000 ft² 93 g / m²
Permeance (WVTR) ASTM E96
Procedure A
0.02 perm
(grains/hr.ft².in Hg)
1.15 ng / N.s
Bursting Strength ASTM D774 65 psi 4.6 kg / cm²
Puncture Resistance ASTM C1136 125 beach units 3.7 Joules
Tensile Strength ASTM C1136 40 lbs/inch width (MD)
35 lbs/inch width (XD)
7.0 kN / m (MD)
6.1 kN / m (XD)
Caliper / Thickness Micrometer 0.009 inch 229 micron
Accelerated Aging 30 Days @
95% RH, 120°F (49°C)
No Corrosion
No Delamination
No Corrosion
No Delamination
Low Temperature Resistance ASTM D1790
-40°F (-40°C)
Remains Flexible
No Delamination
Remains Flexible
No Delamination
High Temperature Resistance 4 hours @
240°F (116°C)
Remains Flexible
No Delamination
Remains Flexible
No Delamination
Water Immersion 24 hours @ 73°F (23°C) No Delamination No Delamination
Mold Resistance ASTM C665 / C1338 No Growth No Growth
Dimensional Stability ASTM D1204 0.25% 0.25%
Light Reflectance ASTM C523 85% 85%

 

FIRE TESTING UL-723 / ASTM E84 CAN ULC-S102M BRITISH STANDARD 476
  Flame Spread Smoke Developed Flame Spread Smoke Developed Parts 6 and 7
Summary Report
Film Exposed 10 10 15 30 Class 0 Surface
Kraft Exposed 15 5 15 45  

 


 